SLA Auxetic Lattice Study Finds Cell Shape Can Quadruple Peak Load
VIT compared star-triangular and re-entrant hexagonal lattices under the same conditions; the best star specimen reached about 2,700 N.
3D Printing Industry
VIT compared star-triangular and re-entrant hexagonal lattices under the same conditions; the best star specimen reached about 2,700 N.
The 200 × 125 × 235 mm system uses 35 µm pixels and automated resin feeding and heating, with shipments scheduled for November 16.